Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Filler/Reinforcement: Long Glass Fiber, 40% Filler by Weight Uses: Appliance Components; Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Connectors; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Household Goods; Hydraulic Applications; Industrial Applications; Pneumatic Applications; Power/Other Tools; Sporting Goods Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |