MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Weston™ 618F Antioxidant
Categories: Other Engineering Material

Material Notes: Product Description: Weston™ 618F phosphate is a phosphite that is a highly effective color and molecular weight stabilizer fro polyolefins, polyesters, elastomers, styrenics, engineering thermoplastics, and adhesive formulations. It also contributes to the thermal and UV stability of these polymers. This product is available in a flake form.

Features:

  • Excellent color stability during processing, fabrication and end use
  • Polymer protection from degradation during processing
  • Reduced discoloration of polymers containing pigments such as TiO2
  • Reduced discoloration of polymers that are stabilized with a sulfur-containing, nickel-organic complex and are processed at high temperatures
  • Synergism when used with light stabilizers such as benzophenones and benzotriazoles

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 - 0.935 g/cc
Bulk Density 0.430 g/cc
Molecular Weight 732 g/mol
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Melting Point 37.0 - 46.0 °C
Flash Point 365 °FPensky-Martens Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.456 - 1.459
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 7.8 - 8.2 %
 
Descriptive Properties
AppearanceWhite Flakes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH515 / 315433

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.