MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Jayflex™ L11P-E Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Jayflex™ adipate plasticizers can be used as a primary plasticizer but, more typically, are used in blends with general-purpose phthalates to improve low-temperature properties. They are effective for extremely low-temperature applications, for resistance to UV light and for food contact applications. Benefits: Greater permanence over Di (2-ethylhexyl) adipate (DEHA), Strong low-temperature performance enhancements, Compatible with all general-purpose phthalates.

Availability: Latin America, North America. Appearance: clear, free of suspended matter (BRCP 4065)

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.951 - 0.957 g/cc
@Temperature 20.0 °C
BRCP 4843
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.10 %BRCP 5053
 
Descriptive Properties
Acidity (% wt)< 0.015(as Phthalic Acid). BRCP 4625
Color, Pt-Co<75BRCP 4273
Ketones, Esters (wt%)99.6BRCP 4630
OdorCharacteristicBRCP 4550

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98992 / 238373

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.