MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Acetron® VMX POM-C FG Food Grade Polyoxymethylene
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Acetron® VMX Polyoxymethylene POM-C FG (Food Grade) is a visual, metal, and x-ray detectable, copolymer acetal grade that provides a unique combination of outstanding mechanical and impact strength, stiffness, and chemical resistance. Due to the addition of specific additives to this formulation, it can be easily traced by conventional metal and x-ray detection systems, making it a favored solution for the global food processing and packaging industry. As a EU 10/2011 and compositional FDA 21 CFR § 177.2470 compliant material, Acetron® VMX POM-C FG allows food processors and packagers to gain the efficiencies that polymer materials provide, while also preventing potential foreign contamination issues that can lead to costly recalls.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.63 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7750 psiASTM D638
Elongation at Break 16 %ASTM D638
Elongation at Yield 13 %ASTM D638
Modulus of Elasticity 496 ksiASTM D638
Flexural Strength 12800 psiASTM D790
Flexural Modulus 515 ksiASTM D790
Compressive Strength 13250 psiASTM D695
Shear Strength 7150 psiASTM D732
Izod Impact, Notched 1.00 ft-lb/inASTM D256
Limiting Pressure Velocity 2190 psi-ft/minat 100 FPM; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+12 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E-831
Melting Point 336 °FDSC, 50°F/min; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 383 °FASTM D648
Flammability, UL94 HB
@Thickness 3.00 mm
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM913 / 291070

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.