MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Clwyd Compounders BIIR Bromobutyl rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Both butyl and halobutyl rubbers provide excellent inflation pressure retention. They are an ideal choice for inner tubes of bicycles, trucks, and industrial and agriculturaltires. In fact, halogenated butyl rubbers are the most widely used butyl rubbers for tire inner liners. Halobutyl rubbers are also used for hoses, seals, membranes, tanklinings, conveyor belts, protective clothing and for consumer products, such as ball bladders for sporting goods. Halobutyls are generally a good choice when good resistance to chemicals, weathering, and ozone is required.

Typical applications:

  • ‘O’ Rings
  • Vacuum seals and membranes
  • Steam hoses
  • Pharmaceutical closures
  • Tire inner tubes
Advantages:
  • High impermeability
  • Better heat resistance
  • Addition of bromine results in faster curing and better adhesion to unsaturated polymers
Disadvantages:
  • Lower resilience

Information provided by CLWYD COMPOUNDERS LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35 - 90
Tensile Strength <= 18.0 MPa
Elongation at Break <= 650 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °CUpper continuous
Minimum Service Temperature, Air -70.0 °Cnon-brittle
 -50.0 °Csealing applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCLWYD022 / 316039

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.