MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX830 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 830 resin is a 30% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade has high stiffness (flexural modulus 8200 MPa), excellent chemical resistance, and high heat resistance. NORYL GTX GTX830 resin is an excellent candidate for a wide variety of applications including automotive under the bonnet applications and water meter housings.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 1.09 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.1 %ISO 62-1
Viscosity 7.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 110 MPaH358/30; ISO 2039-1
Tensile Strength at Break 110 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
Tensile Modulus 7300 MPa1 mm/min; ISO 527
Flexural Strength 170 MPabreak, 2mm/min; ISO 178
Flexural Modulus 6200 MPa2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 45.0 kJ/m²80*10*4; ISO 180/1U
 45.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 60.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179/2C
 7.00 kJ/m²
@Temperature -20.0 °C
ISO 179/2C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.260 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Vicat Softening Point 220 °CRate B/120; ISO 306
 220 °CRate B/50; ISO 306
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Oxygen Index 29 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 290 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 100 °C
Drying Temperature 100 - 110 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82150 / 290097

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.