MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toray 2511 Prepreg System - Resin Properties
Categories: Polymer; Thermoset; Epoxy

Material Notes: This semi-toughened epoxy prepreg system was formulated for better oven cure processing than the #2510 general aviation (AGATE) prepreg system. #2511 provides excellent all-around structural properties with a high wet and dry TG while offering a flexible cure temperature (250°F to 350°F, 121°C to 177°C) with a very low void content. This prepreg system also can be used in industrial and recreational applications.

Information provided by Toray Composite Materials America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.267 g/ccASTM D792
Viscosity >= 700.8 cP
@Temperature 103 °C
ASTM D4440
 >= 8500 cP
@Temperature 103 °C
 >= 10000 cP
@Temperature 110 °C
 >= 10000 cP
@Temperature 93.3 °C
 >= 100000 cP
@Temperature 68.3 °C
 >= 1.00e+6 cP
@Temperature 48.9 °C
Storage Temperature 24.0 °C28 days, Out Life
 <= -12.0 °C
@Temperature -17.8 °C
24 months, Freezer Life
 
Mechanical PropertiesOriginal ValueComments
Fracture Toughness 0.750 ksi-in½KIC; ASTM D5045
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 118 °CWet; ASTM D7028
 162 °CDry; ASTM D7028
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 - 177 °CCure Temp.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY8027 / 265425

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.