MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Corning Valor® Glass Vials
Categories: Ceramic; Glass

Material Notes: Glass vials developed for pharmaceuticals.
  • Eliminates glass delamination: Chemically-durable drug contacting surface with uniform surface chemistry
  • Reduces glass particulate generation: Valor Glass has a low coefficient of friction surface that reduces particulate generation and enhances machinability
  • Resists damage and breakage: Exceptional damage resistance and retained strength throughout processing
  • Enables higher throughput through smoother filling line operations: Valor Glass containers reduce line interventions, enabling lines to run at higher efficiency and higher speeds with improved yields.
  • Low extractable concentrations in a wide range of pHs.
  • Prevents cracks: In laboratory testing, Valor Glass vials provide at least 30x protection against cracks than conventional borosilicate glass vials

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Al2O3 72 - 75 %72 - 75 %Glass Former
B2O3 <= 0.01 %<= 0.01 %Glass Former
CaO+MgO 3 - 4.5 %3 - 4.5 %Property Modifiers
Chlorine, Cl <= 0.01 %<= 0.01 %Fining Agent
Na2O or K2O 10 - 13 %10 - 13 %Fluxes
Other <= 0.01 %<= 0.01 %As2O5; Fining Agent
 0.1 - 1 %0.1 - 1 %SnO2; Fining Agent
SiO2 9 - 12 %9 - 12 %Glass Former
 
Descriptive Properties
Acid Resistance ClassClass S1DIN 12116
Alkali Resistance ClassClass A2ISO 695
Hydrolytic ResistanceHGB1ISO 719
 Type 1Ph. Eur. 3.2.1/USP <660>
Soluble Alkali TestMeets JP 7.01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCORNG995 / 254547

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.