MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Huber Hymod® M9400 SP Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Overall Benefits: Huber Engineered Materials’ Hymod® M9400 SP aluminum hydroxide (ATH) is a vinyl functionalized, precipitated grade developed for peroxide-cured silicone rubber. Everything about this product has been optimized for maximum performance in high-voltage, silicone rubber insulator compositions. The resulting product performs well on the job. Silicone rubber compound containing Hymod® M9400 SP does not stick in the mold. This increases the value of your compound to your customers. They will save money by reducing the number of rejected parts.

Product Advantages: The Hymod®M9400 SP product has a narrow particle size distribution for optimum particle spacing in silicone. Optimum particle spacing in turn provides for maximum resistance to carbon tracking. Aluminum hydroxide has a polar surface, making it difficult to fully disperse in non-polar resins such as silicone rubber. The SP surface treatment reduces surface tension between the ATH and silicone, permitting optimum wet-out and dispersion. Mold fouling can happen if the surface treatment is not optimized for proper level and attachment to the ATH surface. Hymod® M9400 SP ATH will not contribute to mold fouling. Extensive testing has been conducted to ensure that Huber’s production protocol: Delivers precisely the right amount of surface treatment; Yields a superior, treated ATH product free from residual silanols.

Performance: Long-term outdoor performance of silicone rubber in applications such as line post insulators, dead end insulators, suspension insulators and surge arrestors requires hydrophobicity. With the highly consistent surface treatment on Hymod® M9400 SP aluminum hydroxide, the surface is extremely hydrophobic for optimum resistance to environmental water pick-up. A complete product specification is available upon request.

Processability: This precipitated Hymod® M9400 SP aluminum hydroxide product is easy to use as long as processing temperatures stay below the ATH decomposition temperature of 200?C.

Compatibility: Aluminum hydroxide is soluble in strong acids and alkalies.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Volatiles 0.16 %
@Treatment Temp. 105 °C
ASTM D-280
Brightness 96 %Dry Brightness (MgO = 100), ASTM C-110
Particle Size 1.2 µmFQA 3065
Particle Mesh Size 32 Mesh0.01%, FQA 3015
pH 9.0 - 10ASTM D-1208
Specific Surface Area 4.0 m²/gBET
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2.5 - 3.5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1250 ohm-cmASTM D-2448
Dielectric Constant 7.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 - 5.00 µm/m-°C
Specific Heat Capacity 0.800 J/g-°C
Thermal Conductivity 0.840 W/m-K
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.17 %treatment level; FQA 3069
Fe2O3 0.0060 %
Loss on Ignition(%) 34.6 %
@Temperature 550 °C
Na2O 0.025 %soluble
Quartz 0.0050 %
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalityLow Moisture Pick-Up
 Smoke Suppression
Market/Application: ThermoplasticsPolyolefin
Market/Application: ThermosetsRubber & Plastics
Market/Application: Wire and CableWire & Cable Jacketing - PVC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER713 / 300819

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.