MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chosun Refractories GPB-2 Special brick
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.10 g/cc0.112 lb/in³
Porosity 10 %10 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 73.5 MPa10700 psiCold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 µm/m-°C
@Temperature 1000 °C
3.89 µin/in-°F
@Temperature 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 75 %75 %
MgO 9.0 %9.0 %
 
Descriptive Properties
Chemical Analysis(%) SiC+C7
Refractories Under Load(2kg/cm²,T2°C)1,700

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Sikor® S Cordierite
CeramTec Rubalit® 600 Alumina, 48%
CeramTec 433 Alumina, 99.9%
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ Materials Color A Insulating Firebrick (French Grade)

CCHOS077 / 124021

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.