MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi GLASSBEND 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: GLASSBEND is a crystal clear, strong, flexible and easy to print filament for 3D printing. These characteristics, together with the high degree of gloss, very low water absorption, practically no shrinkage or warping, very good interlayer adhesion and flame-retardant properties make it a very special filament. The material is FCA (Food Contact Acceptable) approved. In short, a very diverse filament which can be used for many applications.

Features:

  • 92% light transmission, so very bright
  • Strong and flexible
  • Very good interlayer adhesion
  • No crazing when bent
  • Food Contact Acceptable
  • Almost no ”warping”
Colors: GLASSBEND is available from stock in clear. Other colors on request

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccISO 1183
Filament Diameter 1750 µmTolerance: 50 µm, =95% Roundness
 2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ISO 868
Tensile Strength, Yield 26.0 MPaISO 527
Elongation at Yield 230 %ISO 527
Flexural Modulus 1795 MPaISO 178
Dart Drop, Total Energy 40.0 J
@Thickness 2.18 mm
TE; ASTM 3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 - 235 °CISO 294
Vicat Softening Point 85.0 °CISO 306 B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 92 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 280 °CPrinting Temperature
 
Descriptive Properties
Bed Temp=100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9826 / 301051

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.