MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren LSR 4655 SL Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Silopren LSR 4655 SL is a USP Class VI and ISO10993 biocompatible, two- component self-lubricating liquid silicone rubber for injection molding processes. Silopren LSR 4655 SL cures quickly to form a lubricious surface. Silopren LSR 4655 SL is an excellent candidate to consider for medical device applications such as needle-free access valves, O-rings, stoppers, and other parts requiring assembly. Silopren LSR 4655 SL is a 55 durometer, self-lubricating liquid silicone rubber that has been tested to USP Class VI and ISO 10993 biocompatibility standards. Its design includes a delayed lubricant surface bloom which enables efficient part molding without the mold-fouling seen with other self-lubricating materials. Silopren LSR 4655 SL has a high slip surface as evidenced by a low coefficient of friction after molding, enabling automated assembly of molded components and devices. Silopren LSR 4655 SL can also be formulated to a wide variety of hardnesses via the custom compounding center to meet specific end use requirements. Silopren LSR 4655 SL self-lubricating SL can be considered for a variety of applications that require a lubricious surface including seals, stoppers, needle-free access valves, septums and O-rings.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55
Tensile Strength 8.00 MPa
Elongation at Break 450 %
Tear Strength 45.9 kg(f)/cmDie B.
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9963 / 265778

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.