System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ascend Performance Materials Vydyne® B 25 GF BK EST K1 PA6-GF25
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Glass Fiber Filled
Material Notes:
Vydyne B 25 GF BK EST K1 is standard flow, heat stabilized, 25% glass-fiber reinforced PA6 resin. Available in black, this product is also lubricated for improved machine feed and flow.
Information provided by Ascend Performance Materials.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.32
g/cc
DAM; ISO 1183
Water Absorption
1.9 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium
2.0 %
@Temperature 23.0 °C
DAM; ISO 62
Linear Mold Shrinkage, Flow
0.0050
cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
98.0
MPa
50% RH; ISO 527-2
162
MPa
DAM; ISO 527-2
Elongation at Break
3.3 %
DAM; ISO 527-2
8.1 %
50% RH; ISO 527-2
Tensile Modulus
5100
MPa
50% RH; ISO 527-2
8000
MPa
DAM; ISO 527-2
Flexural Strength
117
MPa
50% RH; ISO 178
217
MPa
DAM; ISO 178
Flexural Modulus
4800
MPa
50% RH; ISO 178
7800
MPa
DAM; ISO 178
Poissons Ratio
0.34
ISO 527-2
Izod Impact, Notched (ISO)
7.50
kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
8.00
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
8.50
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
10.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
11.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
17.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched
60.0
kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
61.0
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
66.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
72.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
76.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
85.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched
8.10
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
8.30
kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
10.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
11.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
15.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
18.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Electrical Properties
Original Value
Comments
Dielectric Strength
24.0
kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
27.0
kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Comparative Tracking Index
<=
450
V
@Thickness 3.00 mm
IEC 60112
>=
450
V
@Thickness 3.00 mm
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
23.0
µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point
220
°C
DAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi)
208
°C
Unannealed; 50% RH; ISO 75-2/B
218
°C
Unannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi)
193
°C
Unannealed; 50% RH; ISO 75-2/A
201
°C
Unannealed; DAM; ISO 75-2/A
Flammability, UL94
HB
@Thickness 1.50 mm
UL 94
HB
@Thickness 3.00 mm
UL 94
Processing Properties
Original Value
Comments
Rear Barrel Temperature
>=
230
°C
Injection
<=
280
°C
Injection
Middle Barrel Temperature
>=
230
°C
Injection
<=
280
°C
Injection
Front Barrel Temperature
>=
230
°C
Injection
<=
280
°C
Injection
Nozzle Temperature
>=
230
°C
Injection
<=
280
°C
Injection
Melt Temperature
>=
230
°C
Injection
<=
280
°C
Injection
Mold Temperature
>=
80.0
°C
Injection
<=
90.0
°C
Injection
Drying Temperature
>=
80.0
°C
Injection
<=
90.0
°C
Injection
Dry Time
>=
3.00
hour
Injection
Descriptive Properties
Additive
Heat Stabilizer
Lubricant
Appearance
Black
Features
Chemical Resistant
Gasoline Resistant
General Purpose
Good Flow
High Heat Resistance
Lubricated
Forms
Pellets
Processing Method
Injection Molding
Region
North America, Europe, Asia Pacific
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PASCE9264 / 287617
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.