MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
En-Door ACR ED-401A PVC Processing Aid
Categories: Other Engineering Material

Material Notes: General Information: ED-401A is a low molecular weight acrylic processing aid. It can be used in rigid PVC formulations to improve the process ability and the surface quality. It can accelerate fusion rate, increase productivity, decrease processing temperature, increased output rates and improved production efficiency.ED-401A has better dispersion, excellent clarity and surface quality for end-use products, superior fusion promotion for rigid and soft PVC.

Application: ED-401A is mainly used in producing PVC transparent sheets, films, etc. The recommended dosage is 1.5-2.5 phr for 100 phr PVC resin

Information provided by En-Door

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.400 - 0.550 g/ccSurface
Volatiles <= 1.0 %
Particle Mesh Size 40 Mesh0.45mm, =98%, Granularity
Viscosity Measurement 2.5 - 3.2[?], Ubbelohde Viscometer
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENDOOR033 / 316667

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.