Compound 4617 is a 60 durometer black colored Neoprene elastomer, it is formulated with molybdenum disulfide to provide internal lubrication. It exhibits good resistance to compression set at moderate temperature. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 BC 615 B14 EO14; 5 BC 615 B14 EO14; 6 BC 615 B14 EO14; 2 BE 615 B14 EO14; 3 BE 615 B14 EO14 Information provided by Pressure Seals Inc. |