Product Description: A soft, black SEBS based thermoplastic elastomer (TPE) compound designed for contact with non-fatty foods. The monomers and additives used to produce this product are listed in the Union List of Authorized Substances of Regulation 10/20/11/EC. Bondable to: PP, EVA, PE Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Block Copolymer; Bondability; Food Contact Acceptable; Soft Agency Ratings: EU 2011/10/EU RoHS Compliance: RoHS Compliant Appearance: Black Forms: Pellets Processing Method: Injection MoldingInformation provided by Elastron |