MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Cyberbond CB 2006 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive

Material Notes: Elastomer and Plastic Series: very fast bonding; good ageing properties and low viscosity. The Elastomer and Plastic Series stands for Cyanoacrylates with extreme good properties in bonding rubber (especially EPDM) and plastics with each other or in combination. The ageing properties of these joints are outstanding. The overall properties made CB 2006 (like CB 2008) to a favourable EPDM bonder. Compared to CB 2008 the viscosity is slightly higher. In addition the low viscosity allows very thin bond layers. CB 2006 should be considered as the first choice in this viscosity range.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Viscosity 15 - 30 cPcone-plate, 160 rpm @ 20 °C
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 725 - 1740 psiNBR-rubber
 1450 - 3770 psisteel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point 85.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 3.00 secSet time, EPDM
 3.00 - 5.00 secSet time, plastic (ABS)
 15.0 - 35.0 secSet time, metal (Steel)
Shelf Life 12.0 Month
 
Descriptive Properties
Base compoundEthyl-2-cyanoacrylate
Colorcolourless, transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL015 / 316806

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.