NORYL APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be electro-statically painted or powder coated without the need for a conductive primer. The resin is injection moldable and only available in black.Information provided by SABIC Innovative Plastics for the Americas. |