MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Beryllium Copper, UNS C17300, TD02 Temper, Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Solution Heat Treated and Cold Worked: 1/2 Hard

Fabrication Properties: Excellent Suitability – Capacity for Being Hot Formed; Good Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Capacity for Being Cold Worked; Fair Suitability – Seam Weld, Butt Weld

Common Fabrication Processes: Blanking; Drawing; Drilling; Forming and Bending; Tapping; Turning

Typical uses: Clips; Connectors; Contact Bridges; Electric Motor Components; Electrical Connectors; Electrical Switch and Relay Blades; Fuse Clips; Navigational Instruments; Relay Parts; Switch Parts; Bolts; Fasteners; Lock Washers; Roll Pins; Screws; Washers; Bellows; Bourdon Tubes; Bushings; Diaphragms; Electrochemical Springs; Flexible Metal Hose; Non Sparking Safety Tools; Pump Parts; Pumps; Rolling Mill Parts; Shafts; Spline Shafts; Springs; Springs, Valve; Welding Equipment; Firing Pins

Applicable Specifications: Bar – MILITARY MIL-C-21657, ASTM B196/B196M; Rod – ASTM B196/B196M, MILITARY MIL-C-21657; Wire – ASTM B197/B197M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.298 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 122 ksi
Tensile Strength, Yield 100 ksi0.2% Offset
Elongation at Break 5.0 %
Tensile Modulus 18500 ksi
Modulus of Rigidity 7300 ksi
Poissons Ratio 0.27Calculated
Machinability 50 %
Forgeability 0.00 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000780 ohm-cm22% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.100 BTU/lb-°F
Thermal Conductivity 62.0 BTU-in/hr-ft²-°F
Melting Point 1590 - 1800 °F
Solidus 1590 °F
Liquidus 1800 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 400 °FStress Relief
Solution Temperature 1425 - 1475 °F
@Time 30.0 sec
Water
Hot-Working Temperature 1200 - 1500 °F
Precipitation Temperature 600 °FAir
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.20 %
Beryllium, Be 1.8 - 2.0 %
Cobalt, Co >= 0.20 %
Copper, Cu 97 - 97.8 %As Balance
Lead, Pb 0.20 - 0.60 %
Silicon, Si <= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC17300x5 / 292835

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.