MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 23518 Ethylene Propylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 23518 is a 50 durometer black colored EPDM elastomer, it is formulated with Teflon to provide internal lubrication. It exhibits good resistance to heat and water. It will remain non brittle at very low temperatures. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 AA 520 A13 F17 EA14; 3 AA 520 B13 B33 F17 EA14; 4 AA 520 A13 B13 B33 F17 EA14; 5 AA 520 A13 B13 B33 F17 EA14; 2 BA 520 F17; 3 BA 520 A14 B13 F17 F19; 4 BA 520 A14 F17; 5 BA 520 F17 F19; 3 CA 510 A25 B44 B35 F17 F18 EA14; 4 CA 510 A25 B44 F17 F18 F19 EA14; 2 DA 520 F19 G11 G21 EA14

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53
 47
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 51
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 59
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 62
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 62
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 65
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 65
@Temperature 150 °C,
Time 252000 sec
Heat Aged
Tensile Strength 2133 psi
 2310.04 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 2310.04 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 2410.3 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 2410.3 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 2465.7 psi
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 2472.1 psi
@Temperature 100 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 638 %
 650.1 %
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 662.9 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 662.9 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 675 %
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 687.8 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 687.8 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
100% Modulus 137 psi
Tear Strength 117 pliDie B
Compression Set 14.8 %
@Temperature 100 °C,
Time 79200 sec
Solid
 15.3 %
@Temperature 100 °C,
Time 79200 sec
Plied
 18.4 %
@Temperature 70.0 °C,
Time 79200 sec
Solid
 22.6 %
@Temperature 70.0 °C,
Time 79200 sec
Plied
 23.5 %
@Temperature 100 °C,
Time 252000 sec
Plied
 23.8 %
@Temperature 125 °C,
Time 79200 sec
Plied
 44.3 %
@Temperature 150 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -103 °F
Shrinkage 1.7 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL221 / 318431

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.