MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraiburg TPE THERMOLAST® TF5BNB Thermoplastic Elastomer, natural  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:
    Typical Markets / Application Sectors:
  • Packaging Food
  • Personal Care & Baby Care
  • Stationaries
  • Electric Household Appliance
  • Household goods

    Application Examples:
  • Anti-slip elements
  • Functional elements
  • Handles
  • Design elements
  • Seals
  • Soft grip zones
  • Writing utensil soft touch

    Material Advantages:
  • Excellent physical properties
  • Extremely flexible
  • Easy to color
  • BfR, FDA, 2002/72/EC and EN 71/3 compliant
  • Smooth surface
  • Adhesion to PP
  • Service temperature: -40° to +100°C (dynamic stress: up to 80°C)
  • With many prevalent methods weldable
  • Recyclable
  • Halogen-free

Information provided by Kraiburg TPE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccDIN EN ISO 1183-1:2004
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55DIN 53505 / ISO 868
Tensile Strength at Break 7.50 MPaDIN 53504 / ISO 37
Elongation at Break 790 %DIN 53504 / ISO 37
Graves Tear Strength 17.0 kN/mDIN ISO 34-1 Method B (b)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
ColorNatural

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboCoat 8508-1 Heavy-Duty Epoxy Paint
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
Claude Bamberger Bamberko® 9016 Purge Compound
Top Polymer Topolymer® M-601J TPE
Overview of materials for Styrenic Elastomer (TES)

PKRAIB414 / 101787

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.