MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® A 25 GF BLACK TT/C PA66-GF25
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: VYDYNE A 25 GF BLACK TT/C is a glass fiber reinforced with 25% glass fiber PA66. It is suitable for extrusion and thermal break applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 1.4 %
@Temperature 23.0 °C
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 135 MPaDAM; ISO 527-2
Elongation at Break 3.5 %DAM; ISO 527-2
Tensile Modulus 7800 MPaDAM; ISO 527-2
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index <= 575 V
@Thickness 3.00 mm
IEC 60112
 >= 575 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 240 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 230 °CUnannealed; DAM; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.800 mm
UL 94
 HB
@Thickness 1.60 mm
UL 94
Glow Wire Flammability Index 650 °C
@Thickness 0.200 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Zone 1 >= 255 °CExtrusion
 <= 275 °CExtrusion
Zone 2 >= 255 °CExtrusion
 <= 285 °CExtrusion
Zone 3 >= 255 °CExtrusion
 <= 295 °CExtrusion
Zone 4 >= 255 °CExtrusion
 <= 300 °CExtrusion
Zone 5 >= 255 °CExtrusion
 <= 310 °CExtrusion
Die Temperature 255 - 275 °CExtrusion
Melt Temperature >= 255 °CExtrusion
 <= 275 °CExtrusion
Drying Temperature >= 85.0 °CInjection
 <= 95.0 °CInjection
Dry Time >= 3.00 hourInjection
 
Descriptive Properties
AppearanceBlack
FeaturesGeneral Purpose
 Good Impact Strength
 Good Processability
 Good Rigidity
 Good Stiffness
 Good Toughness
 High Viscosity
FormsPellets
Processing MethodProfile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8493 / 318010

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.