MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical SÉETEC M1650 PP Block copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Applications: Food container (Coffee cup)

Typical properties: SÉETEC M1650 is polypropylene block copolymer for injection molding applications. It exhibits an excellent stiffness, good impact resistance and is nucleated for high productivity by cycle time reduction. This grade meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength, Yield 26.0 MPa3770 psi50 mm/min; ASTM D638(
Elongation at Break 100 %100 %50 mm/min; ASTM D638
Flexural Modulus 1.60 GPa232 ksi28 mm/min; ASTM D790(
Izod Impact, Notched  0.390 J/cm
@Temperature -20.0 °C
0.731 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.781 J/cm
@Temperature 23.0 °C
1.46 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FASTM D648
Vicat Softening Point 151 °C
@Load 1.00 kg
304 °F
@Load 2.20 lb
ASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4920WZ Polypropylene, Impact Copolymer
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
LG Chemical SÉETEC M1850 PP Block copolymer
LyondellBasell Clyrell EC 390T Polypropylene
LG Chemical SÉETEC M1885 PP Block copolymer

PLHCHEM9884 / 239400

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.