Physical Properties | Original Value | Comments |
---|
Density | 0.980 g/cc |
| 1.16 g/cc |
| 1.17 g/cc |
Viscosity | 116 cP @Temperature 22.0 °C |
| 350 cP @Temperature 48.9 °C |
| 1291 cP @Temperature 29.0 °C |
| 1400 cP @Temperature 29.4 °C |
| 1974 cP @Temperature 25.0 °C |
| 2599 cP @Temperature 22.0 °C |
| 4000 cP @Temperature 15.6 °C |
| 10000 cP @Temperature 22.0 °C |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Shore D | 86 @Treatment Temp. 60.0 °C, Time 28800 sec |
| 86 @Treatment Temp. 82.0 °C, Time 28800 sec |
| 91 @Treatment Temp. 60.0 °C, Time 57600 sec |
Tensile Strength | 10200 psi @Treatment Temp. 60.0 °C, Time 28800 sec |
| 10200 psi @Treatment Temp. 60.0 °C, Time 57600 sec |
| 10300 psi @Treatment Temp. 82.0 °C, Time 28800 sec |
Elongation at Break | 4.8 % @Treatment Temp. 60.0 °C, Time 28800 sec |
| 6.2 % @Treatment Temp. 60.0 °C, Time 57600 sec |
| 6.3 % @Treatment Temp. 82.0 °C, Time 28800 sec |
Tensile Modulus | 405000 psi |
| 458000 psi |
| 483000 psi |
Flexural Strength | 17700 psi @Treatment Temp. 60.0 °C, Time 28800 sec |
| 17700 psi @Treatment Temp. 60.0 °C, Time 57600 sec |
| 17700 psi @Treatment Temp. 82.0 °C, Time 28800 sec |
Flexural Modulus | 421000 psi @Treatment Temp. 82.0 °C, Time 28800 sec |
| 484000 psi @Treatment Temp. 60.0 °C, Time 28800 sec |
| 484000 psi @Treatment Temp. 60.0 °C, Time 57600 sec |
Compressive Yield Strength | 14100 psi @Treatment Temp. 60.0 °C, Time 28800 sec |
| 14100 psi @Treatment Temp. 60.0 °C, Time 57600 sec |
| 14100 psi @Treatment Temp. 82.0 °C, Time 28800 sec |
|
Thermal Properties | Original Value | Comments |
---|
Deflection Temperature at 0.46 MPa (66 psi) | 162 °F @Treatment Temp. 60.0 °C, Time 28800 sec |
| 174 °F @Treatment Temp. 60.0 °C, Time 57600 sec |
| 208 °F @Treatment Temp. 82.0 °C, Time 28800 sec |
Glass Transition Temp, Tg | 224 °F |
| 167 °F @Treatment Temp. 60.0 °C, Time 28800 sec |
| 174 °F @Treatment Temp. 60.0 °C, Time 57600 sec |
| 181 °F @Treatment Temp. 60.0 °C, Time 28800 sec |
| 188 °F @Treatment Temp. 60.0 °C, Time 57600 sec |
| 208 °F @Treatment Temp. 82.0 °C, Time 28800 sec |
| 210 °F @Treatment Temp. 60.0 °C, Time 28800 sec |
| 215 °F @Treatment Temp. 82.0 °C, Time 28800 sec |
| 219 °F @Treatment Temp. 60.0 °C, Time 57600 sec |
| 241 °F @Treatment Temp. 82.0 °C, Time 28800 sec |
|
Processing Properties | Original Value | Comments |
---|
Cure Time | 12.0 - 14.0 hour |
Pot Life | 94.0 - 116 min @Load 0.500 kg, Temperature 29.0 °C |
| 123 - 151 min @Load 0.500 kg, Temperature 25.0 °C |
| 142 - 174 min @Load 0.150 kg, Temperature 29.0 °C |
| 162 - 198 min @Load 0.500 kg, Temperature 22.0 °C |
| 187 - 229 min @Load 0.150 kg, Temperature 25.0 °C |
| 223 - 273 min @Load 0.150 kg, Temperature 22.0 °C |
Working Life | 8.00 - 9.00 hour |
Shelf Life | 24.0 Month |
| 36.0 Month |
|
Descriptive Properties |
---|
Mix ratio | 100:23.4–100:32.3 |
| 100:27.8 |
| 100:28.0–100:38.7 |
| 100:33.3 |
| 3.00:1 |
| 3.5:1 |
| 3.57:1–2.58:1 |
| 4.28:1–3.10:1 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.