MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Dow™ 722 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: DOW LDPE 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist food packaging, sugar pouches, lidding stock and medical packaging. DOW LDPE extrusion coating resins provide optimal neck-in and draw-down performance with minimal taste/odor contribution. DOW Polyethylene 722 is broad molecular weight distribution homopolymer designed to offer good impact strength and crack resistance, with excellent flexibility. The resin has good processability over a wide range of molding conditions.
  • Typical applications include caps/closures
  • Good impact, ESCR with excellent flexibility

Complies with: US FDA 21 CFR 177.1520©2.2; US FDA DMF; EU No 10/2011; Canadian HPFB No Objection (with Limitations). Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©2.2; Canadian HPFB No Objection

Form: Pellets

Processing Method: Extrusion Blow Molding; Injection Blow Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D792
Water Vapor Transmission 1.70 g/100 in²/dayASTM F1249
ESCR 100% Igepal® <= 1.0 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 2.00 in
@Temperature 321 °C
1.0 mil
Coating Weight 4.40 lb/ream
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 43Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 1400 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 1200 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 500 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 4.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 34000 psi2% Secant, Molded and tested in accordance with ASTM D4976; ASTM D790B
Tensile Impact Strength 130 ft-lb/in²Type S; ASTM D1822
Coefficient of Friction 0.60ASTM D1894
Heat Seal Strength Initiation Temperature 221 °F
 
Thermal PropertiesOriginal ValueComments
Melting Point 224 °F
Crystallization Temperature 204 °FPeak
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °FUnannealed, Molded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 190 °FASTM D1525
Brittleness Temperature -76.0 °FMolded and tested in accordance with ASTM D4976; ASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 600 - 630 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF473 / 311166

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.