Product Description: Modified PPE; Unreinforced non-Flame retardant; Please contact us for drinking water standards information Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Drinking Water Contact Acceptable Processing Method: Injection Molding Part Marking Code (ISO 11469): PPE+PS Information provided by Asahi Kasei Corporation |