MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

American Elements Iron Oxide Nanopowder
Categories: Ceramic; Oxide

Material Notes: General Description

Iron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Iron Oxide Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7 m 2 /g. Nano Iron Oxide Particles are also available in ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Iron Oxide Nanocrystals include in magnetic resonance to provide a contrast at very low concentrations in the nanomolar range for studying tumors, as Magnetic Nanoparticles capable of killing malignant cancer cells, as a targeted delivery vehicle and as a drug delivery coating for nanoscale anticancer drugs, for magnetic data storage and magnetic resonance imaging (MRI) and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties.

Key Words: Formula: Fe2O3; CAS Number: 1309-37-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.020 - 0.040 µm0.020 - 0.040 µm
 0.10 µm0.10 µm
Specific Surface Area 7.0 m²/g7.0 m²/g
 30 - 50 m²/g30 - 50 m²/g
Molecular Weight 159.69 g/mol159.69 g/mol
 
Descriptive Properties
AppearanceBrown Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Augite (Iron-Magnesium Silicate)
Iron (II) Tungstate, FeWO4
Ferrite 1, Sintered Iron-Barium Oxide Hard Magnetic Material
American Elements Cobalt Iron Nanopowder
Iron, Fe

EJAMER44 / 5527

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.