MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Mercaptobenzothiazole
Material Notes: Solubility: less than 1 mg/mL at 66° F; 6.58e-04 M; In water at 25 ?, 51 mg/L (pH 5), 118 mg/L (pH 7), 900 mg/L (pH 9); In pure water, 120 mg/L at 24 ?; in buffered creek water at 24 ?, 190 mg/L (pH 6.5), 230 mg/l (pH 7.5), 260 mg/L (pH 8.5); Solubility at 25 ? (g/100 mL) in alcohol: 2.0; ether 1.0; acetone 10.0; benzene 1.0; carbon tetrachloride <0.2; naphtha <0.5. Moderately soluble in glacial acetic acid. Soluble in alkalies and alkali carbonate solutions; Soluble in dilute caustic soda, alcohol, acetone, benzene, chloroform; insoluble in water and gasoline.; SOL IN HOT ACETIC ACID; MORE SOL IN CRUDE SWEAT THAN IN WATER; 0.12 mg/mL at 24 ?; Solubility in water, g/100ml at 20 ?: 0.01 (very poor)

Alfa Chemistry Materials product group: Polymer Science

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solubility in Water <= 0.10 %
@Temperature 18.9 °C
<= 0.10 %
@Temperature 66.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA67367 / 304099

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.