MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

INEOS Styrolution Polystyrol 158 K GR 2 PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; for transparent, impact resistant applications in blends with Styrolux. High heat resistance GPPS, High transparency. Applications: Replacement of SAN in several application like water filter containers, pen parts etc., Transparent sheet for Showcases & displays, consumer electronics, household application, photo frames, building material etc., Ideal material for physically or chemically foamed high-quality foamed articles, such as foam containers, labels or profiles (PSP /XPS), In blends with high impact polystyrene or Styrolux, Injection molded articles

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³with external lubricant
Density 1.048 g/cc0.03786 lb/in³ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inISO 294-4
Melt Flow  3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiISO 2039-1
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Strength 103 MPa14900 psiISO 178
Izod Impact, Notched (ISO) 2.50 kJ/m²
@Temperature 23.0 °C
1.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 3300 MPa479000 psiISO 899
Tensile Creep Modulus, 1000 hours 2600 MPa377000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant  2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
IEC 60250
 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 135 kV/mm3430 kV/inShort time, 1.5 mm; IEC 60243-1
Dissipation Factor  0.000050
@Frequency 1e+6 Hz
0.000050
@Frequency 1e+6 Hz
IEC 60250
 0.000090
@Frequency 100 Hz
0.000090
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  101 °C
@Load 5.10 kg
214 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 106 °C
@Load 1.02 kg
223 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 108 °C
@Load 1.02 kg
226 °F
@Load 2.25 lb
B/1 120C/h; ASTM D 1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 260 °C356 - 500 °FISO 294
Mold Temperature 10.0 - 60.0 °C50.0 - 140 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
ColorCrystal Clear 00013
Commercial StatusEurope
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Polystyrol 143 E GR 2 PS
BASF Polystyrol® 143 E Polystyrene (Europe)
INEOS Styrolution PS-148G Polystyrene
INEOS Styrolution Polystyrol 168 N GR 2 PS
INEOS Styrolution PS 147F GPPS

PBASG0623 / 132256

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.