MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PA66-GF50-0111P7.5/11 PA666, 50% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 40% Glass Fiber Reinforced

Material Notes: Material code according to ISO 1043-1: PA66
PA66/6 copolymer with 50% ash content - 7.5mm

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 260 MPa37700 psi5mm/min; ISO 527-2/1A
Tensile Strength 150 MPa
@Temperature 80.0 °C
21800 psi
@Temperature 176 °F
ISO 527-1, -2
Elongation at Break 2.2 %2.2 %5mm/min; ISO 527-2/1A
 2.8 %
@Temperature 80.0 °C
2.8 %
@Temperature 176 °F
ISO 527-1, -2
Tensile Modulus 16.6 GPa2410 ksi1mm/min; ISO 527-2/1A
 8.05 GPa
@Temperature 80.0 °C
1170 ksi
@Temperature 176 °F
ISO 527-1, -2
Flexural Strength 380 MPa55100 psiISO 178
 260 MPa
@Temperature 80.0 °C
37700 psi
@Temperature 176 °F
ISO 178
Flexural Modulus 13.5 GPa1960 ksiISO 178
 9.50 GPa
@Temperature 80.0 °C
1380 ksi
@Temperature 176 °F
ISO 178
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179/1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eA
 4.20 J/cm²
@Temperature -30.0 °C
20.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 °C464 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 220 °C428 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 80.0 °C158 - 176 °F
 90.0 - 120 °C194 - 248 °FCavity temperature
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 280 - 285 °C536 - 545 °F
Zone 2 280 - 290 °C536 - 554 °F
Zone 3 290 - 300 °C554 - 572 °F
Zone 4 300 - 310 °C572 - 590 °F
Die Temperature 310 - 320 °C590 - 608 °F
Melt Temperature 310 - 320 °C590 - 608 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content 0.15 %0.15 %Necessary low maximum residual
Injection Pressure 120 - 150 MPa17400 - 21800 psi
Hold Pressure 50.0 - 80.0 MPa7250 - 11600 psi
Back Pressure 3.00 MPa435 psi
Screw Speed  25 rpm
@Diameter 75.0 mm
25 rpm
@Diameter 2.95 in
 35 rpm
@Diameter 55.0 mm
35 rpm
@Diameter 2.17 in
 50 rpm
@Diameter 40.0 mm
50 rpm
@Diameter 1.57 in
Hot-Working Temperature 300 - 315 °C572 - 599 °F
 
Descriptive Properties
Injection speedmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® BG-50 FC PA6-GF50
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Celanese Celstran® PA66-GF50-20 PA66, 50% Glass Reinforced
Celanese Celstran® PA66-GF50-20 AD3007 Nylon 66, 50% Glass Reinforced
Celanese Celstran® PA66-GF50-07 Nylon 66, 50% Glass Reinforced

PHCR149 / 158718

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.