MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek Tungsten Carbide, WC
Categories: Ceramic; Carbide

Material Notes: Information provided by CoorsTek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.9 g/cc0.538 lb/in³ASTM C20
Water Absorption 0.00 %0.00 %ASTM C373
Particle Size 2.0 µm2.0 µmAverage Crystal Size - Thin Section Test
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 627 GPa90900 ksiASTM C848
Flexural Strength 1930 MPa280000 psiASTM F417
Compressive Strength 5000 MPa725000 psiASTM C773
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  <= 1000 ohm-cm
@Temperature 500 °C
<= 1000 ohm-cm
@Temperature 932 °F
 <= 1000 ohm-cm
@Temperature 1000 °C
<= 1000 ohm-cm
@Temperature 1830 °F
 <= 1000 ohm-cm
@Temperature 25.0 °C
<= 1000 ohm-cm
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.10 µm/m-°C
@Temperature 25.0 - 1000 °C
2.83 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C372
Thermal Conductivity 100 W/m-K694 BTU-in/hr-ft²-°FASTM C408
Maximum Service Temperature, Air 1000 °C1830 °FNo Load
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 0.00 %0.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
Tungsten Carbide, W2C
H.C. Starck Amperit® 512.074 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12
Goodfellow Tungsten Carbide/Cobalt
CoorsTek ACI-Ni6 Tungsten Carbide

CZ3C3 / 2752

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.