MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1409 has an excellent balance of mechanical properties and is easy to injection mould.

Applications: Injection moulded housings, boxes and technical parts. PRE-ELEC® PA 1409 is well suited for applications where the good mechanical properties of polyamide are required.

Processing: PRE-ELEC® PA 1409 compound can be processed in the injection moulding machines using normal processing conditions as with polyamide.
Test Specimen: 10[mm] wide moulded rod

Information from Premix OY

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Thickness 102 microns4.00 mil
Linear Mold Shrinkage 0.016 - 0.022 cm/cm0.016 - 0.022 in/inISO 294-4
Melt Flow  8.5 g/10 min
@Load 5.00 kg,
Temperature 275 °C
8.5 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 43 g/10 min
@Load 10.0 kg,
Temperature 275 °C
43 g/10 min
@Load 22.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ISO 868
Tensile Strength 58.0 MPa8410 psiISO 527
Tensile Strength, Yield 59.0 MPa8560 psiISO 527
Elongation at Break 29 %29 %ISO 527
Elongation at Yield 8.0 %8.0 %ISO 527
Flexural Modulus 2.90 GPa421 ksiISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Thickness 4.00 mm,
Temperature -20.0 °C
1.90 ft-lb/in²
@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
 11.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
5.23 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO)  51.0 kJ/m²
@Thickness 4.00 mm,
Temperature -20.0 °C
24.3 ft-lb/in²
@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
 NB
@Thickness 4.00 mm,
Temperature 23.0 °C
NB
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  NB
@Thickness 102 mm,
Temperature 23.0 °C
NB
@Thickness 4.00 in,
Temperature 73.4 °F
ISO 179
 NB
@Thickness 102 mm,
Temperature -20.0 °C
NB
@Thickness 4.00 in,
Temperature -4.00 °F
ISO 179
Charpy Impact, Notched  0.700 J/cm²
@Thickness 102 mm,
Temperature -20.0 °C
3.33 ft-lb/in²
@Thickness 4.00 in,
Temperature -4.00 °F
ISO 179
 1.00 J/cm²
@Thickness 102 mm,
Temperature 23.0 °C
4.76 ft-lb/in²
@Thickness 4.00 in,
Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmISO D-257
Surface Resistance <= 1e+05<= 1e+05ISO IEC 61340-5-1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °F75/Method Bf
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °F75/Method Af
Vicat Softening Point 190 °C374 °FISO 306/B50
 218 °C424 °FISO 306/A50
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 280 °C428 - 536 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °FPre-drying
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 60.0 - 80.0 MPa8700 - 11600 psi
Shelf Life 12.0 Month12.0 MonthNormal Storing Conditions
 
Descriptive Properties
Injection SpeedModerate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Premix Thermoplastics PRE-ELEC® PC/ABS 1420
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound

PPRELZ017 / 122152

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.