MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polyamide-Imide, Glass Filled
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.58 - 1.90 g/cc0.0571 - 0.0686 lb/in³Average value: 1.65 g/cc Grade Count:7
Water Absorption 0.200 - 0.520 %0.200 - 0.520 %Average value: 0.289 % Grade Count:6
Water Absorption at Saturation 1.30 - 1.50 %1.30 - 1.50 %Average value: 1.45 % Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 85.0 - 90.085.0 - 90.0Average value: 88.3 Grade Count:3
Hardness, Rockwell M 116 - 128116 - 128Average value: 123 Grade Count:3
Hardness, Shore D 90.0 - 92.090.0 - 92.0Average value: 90.7 Grade Count:3
Tensile Strength, Ultimate 79.3 - 221 MPa11500 - 32100 psiAverage value: 149 MPa Grade Count:7
Elongation at Break 2.00 - 4.00 %2.00 - 4.00 %Average value: 2.87 % Grade Count:6
Modulus of Elasticity 6.21 - 14.5 GPa900 - 2100 ksiAverage value: 9.00 GPa Grade Count:6
Flexural Yield Strength 138 - 333 MPa20000 - 48300 psiAverage value: 207 MPa Grade Count:6
 181 - 181 MPa
@Temperature 232 - 232 °C
26300 - 26300 psi
@Temperature 450 - 450 °F
Average value: 181 MPa Grade Count:1
Flexural Modulus 5.66 - 13.8 GPa821 - 2000 ksiAverage value: 8.38 GPa Grade Count:6
 9.86 - 9.86 GPa
@Temperature 232 - 232 °C
1430 - 1430 ksi
@Temperature 450 - 450 °F
Average value: 9.86 GPa Grade Count:1
Compressive Yield Strength 40.0 - 345 MPa5800 - 50000 psiAverage value: 185 MPa Grade Count:6
Compressive Modulus 3.79 - 7.93 GPa550 - 1150 ksiAverage value: 5.24 GPa Grade Count:5
Izod Impact, Notched 0.374 - 1.07 J/cm0.700 - 2.00 ft-lb/inAverage value: 0.609 J/cm Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+13 - 1.00e+18 ohm1.00e+13 - 1.00e+18 ohmAverage value: 2.00e+17 ohm Grade Count:5
Dielectric Constant 3.80 - 6.303.80 - 6.30Average value: 4.45 Grade Count:5
Dielectric Strength 17.7 - 33.0 kV/mm450 - 838 kV/inAverage value: 25.6 kV/mm Grade Count:6
Dissipation Factor 0.00500 - 0.05000.00500 - 0.0500Average value: 0.0210 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.6 - 46.8 µm/m-°C7.00 - 26.0 µin/in-°FAverage value: 28.9 µm/m-°C Grade Count:7
Thermal Conductivity 0.360 - 0.360 W/m-K2.50 - 2.50 BTU-in/hr-ft²-°FAverage value: 0.360 W/m-K Grade Count:4
Maximum Service Temperature, Air 250 - 270 °C482 - 518 °FAverage value: 260 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 268 - 282 °C515 - 540 °FAverage value: 276 °C Grade Count:6
Glass Transition Temp, Tg 275 - 280 °C527 - 536 °FAverage value: 277 °C Grade Count:4
Flammability, UL94 V-0V-0Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyamide-Imide, Molded
Mitsubishi Chemical Advanced Materials Duratron® T5530 PAI Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet)
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Polyimide
Mitsubishi Chemical Advanced Materials Nylatron® SLG-FDA PA6 (ASTM Data Sheet)

O2810 / 78114

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.