MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

APCM DA 409U/S2-Glass Unidirectional Epoxy Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DA409U/S2-glass is a tough, versatile, modified epoxy resin prepreg that cures at 250ºF. The S-2 glass is a Zentron High Strength fiber. Standard weight is 260g/m2 with a 38% resin content. Other weights and resin contents available upon request.

Cure Cycle: Press cured for one hour at 250ºF and 50 psi pressure

Information provided by Adhesive Prepegs for Composite Manufacturers, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1250 MPa181000 psiASTM D3039
Flexural Strength 772 MPa112000 psiASTM D790
Flexural Modulus 28.3 GPa4100 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
1.00 hour
@Pressure 50.0 psi,
Temperature 250 °F
Gel Time 12.0 min
@Temperature 121 °C
12.0 min
@Temperature 250 °F
Shelf Life  0.660 Month
@Temperature 23.9 °C
0.660 Month
@Temperature 75.0 °F
 6.00 Month
@Temperature 4.44 °C
6.00 Month
@Temperature 40.0 °F
 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Resin Content42%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
APCM DA 4518U/E-Glass Unidirectional E-Glass Epoxy Prepreg
Arlon Electronic Materials 47N Quick Cure Epoxy Low-Flow Prepreg
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
Solvay CYCOM® 950 Epoxy Prepreg with Hy-E Std/950 Unidirectional Tape and Roving
Aluminum 5052-H32

PAPCM004 / 187017

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.