PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over the shelf life of the product. This provides consistent performance. The product adheres to a variety of surfaces including steel, aluminum, galvanized steel, plastics and elastomers. Features and Benefits: - Provides better impact and peel strength
- Bonds in 20-30 seconds to most surfaces
- Color is suitable for matching dark surfaces
- Material is capable of curing through gaps as large as 0.020 inches
Soluble In Nitroethane, Methyl Ethyl Ketone, Acetone. Information provided by Permabond. |