MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NanoScale NanoActive® Zinc Oxide  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduced particle sizes (the volume weighted mean is below 0.3 µm).

Applications: Applications include catalysts and catalyst supports, cosmetic and skin care market, paints and coatings, solar cells, transparent UV resistant coatings, and varistors.

Information provided by NanoScale

Composition based on metal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³
Density 5.60 g/cc0.202 lb/in³
Moisture Absorption <= 2.0 %<= 2.0 %
Loss On Ignition <= 4.0 %<= 4.0 %
Particle Size 4.0 µm4.0 µmmean aggregate size
Specific Surface Area >= 70 m²/g>= 70 m²/gBET
Pore Size 0.0170 microns0.000669 milAverage Diameter
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn >= 99 %>= 99 %
 
Descriptive Properties
Appearance / ColorOff-White Powder
Crystallite Size= 10 nm
Minimum Total Pore Volume cc/g0.2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc Oxide, ZnO, Cubic
Zinc Oxide, ZnO, (Zincite)
Arkema Evatane® 1350 VN 5 Ethylene Vinyl Acetate
Arkema Evatane® 1080 VN 5 Ethylene Vinyl Acetate
Arkema Evatane® 1005 VN 3 Ethylene Vinyl Acetate

CNANO08 / 1670

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.