MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.84 g/cc0.0434 - 0.0665 lb/in³Average value: 1.70 g/cc Grade Count:41
 1.47 - 1.60 g/cc
@Temperature 260 - 260 °C
0.0531 - 0.0578 lb/in³
@Temperature 500 - 500 °F
Average value: 1.54 g/cc Grade Count:2
Filler Content 45.0 - 55.0 %45.0 - 55.0 %Average value: 48.8 % Grade Count:8
Water Absorption 0.000 - 0.400 %0.000 - 0.400 %Average value: 0.191 % Grade Count:11
Moisture Absorption at Equilibrium 0.0300 - 0.500 %0.0300 - 0.500 %Average value: 0.159 % Grade Count:15
Water Absorption at Saturation 0.200 - 0.500 %0.200 - 0.500 %Average value: 0.357 % Grade Count:7
Maximum Moisture Content  0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.00100 - 0.00800 cm/cm0.00100 - 0.00800 in/inAverage value: 0.00258 cm/cm Grade Count:28
 0.00300 - 0.00300 cm/cm
@Temperature 80.0 - 80.0 °C
0.00300 - 0.00300 in/in
@Temperature 176 - 176 °F
Average value: 0.00300 cm/cm Grade Count:1
Linear Mold Shrinkage, Transverse 0.00200 - 0.0140 cm/cm0.00200 - 0.0140 in/inAverage value: 0.00764 cm/cm Grade Count:17
 0.0110 - 0.0110 cm/cm
@Temperature 80.0 - 80.0 °C
0.0110 - 0.0110 in/in
@Temperature 176 - 176 °F
Average value: 0.0110 cm/cm Grade Count:1
Melt Flow 2.00 - 30.0 g/10 min2.00 - 30.0 g/10 minAverage value: 9.09 g/10 min Grade Count:19
Ash 47.0 - 52.0 %
@Temperature 625 - 625 °C
47.0 - 52.0 %
@Temperature 1160 - 1160 °F
Average value: 49.5 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 40.0 - 180 MPa5800 - 26100 psiAverage value: 147 MPa Grade Count:38
 45.0 - 90.0 MPa
@Temperature 60.0 - 150 °C
6530 - 13100 psi
@Temperature 140 - 302 °F
Average value: 65.0 MPa Grade Count:1
Tensile Strength, Yield 130 - 166 MPa18900 - 24100 psiAverage value: 146 MPa Grade Count:5
Elongation at Break 1.00 - 4.00 %1.00 - 4.00 %Average value: 1.93 % Grade Count:40
 2.50 - 3.00 %
@Temperature 60.0 - 150 °C
2.50 - 3.00 %
@Temperature 140 - 302 °F
Average value: 2.75 % Grade Count:1
Modulus of Elasticity 4.10 - 18.7 GPa595 - 2710 ksiAverage value: 15.1 GPa Grade Count:33
 4.50 - 10.0 GPa
@Temperature 60.0 - 150 °C
653 - 1450 ksi
@Temperature 140 - 302 °F
Average value: 6.93 GPa Grade Count:1
Flexural Yield Strength 68.0 - 285 MPa9860 - 41300 psiAverage value: 221 MPa Grade Count:24
Flexural Modulus 4.61 - 18.2 GPa668 - 2640 ksiAverage value: 13.2 GPa Grade Count:27
Poissons Ratio 0.3300.330Average value: 0.330 Grade Count:3
Izod Impact, Notched 0.640 - 2.67 J/cm1.20 - 5.00 ft-lb/inAverage value: 1.09 J/cm Grade Count:13
Izod Impact, Unnotched 5.34 - 9.61 J/cm10.0 - 18.0 ft-lb/inAverage value: 7.47 J/cm Grade Count:4
Izod Impact, Notched (ISO) 6.00 - 30.0 kJ/m²2.86 - 14.3 ft-lb/in²Average value: 12.5 kJ/m² Grade Count:10
 9.00 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
4.28 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 9.67 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 33.0 - 80.0 kJ/m²15.7 - 38.1 ft-lb/in²Average value: 52.0 kJ/m² Grade Count:3
 43.0 - 43.0 kJ/m²
@Temperature -30.0 - -30.0 °C
20.5 - 20.5 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 43.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.20 - 7.00 J/cm²10.5 - 33.3 ft-lb/in²Average value: 5.57 J/cm² Grade Count:20
 4.00 - 6.90 J/cm²
@Temperature -30.0 - -20.0 °C
19.0 - 32.8 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 5.95 J/cm² Grade Count:14
Charpy Impact, Notched 0.700 - 3.20 J/cm²3.33 - 15.2 ft-lb/in²Average value: 1.21 J/cm² Grade Count:27
 0.310 - 1.30 J/cm²
@Temperature -30.0 - -20.0 °C
1.48 - 6.19 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 1.05 J/cm² Grade Count:12
Tensile Creep Modulus, 1 hour 12500 - 15000 MPa1.81e+6 - 2.18e+6 psiAverage value: 14200 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 9500 - 11600 MPa1.38e+6 - 1.68e+6 psiAverage value: 10400 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 7.00e+12 - 1.00e+17 ohm-cm7.00e+12 - 1.00e+17 ohm-cmAverage value: 1.02e+16 ohm-cm Grade Count:21
Surface Resistance 1.00e+13 - 4.00e+16 ohm1.00e+13 - 4.00e+16 ohmAverage value: 4.80e+15 ohm Grade Count:14
Dielectric Constant 3.20 - 4.903.20 - 4.90Average value: 4.18 Grade Count:10
Dielectric Strength 16.0 - 100 kV/mm406 - 2540 kV/inAverage value: 32.2 kV/mm Grade Count:17
Dissipation Factor 0.00120 - 0.02600.00120 - 0.0260Average value: 0.0121 Grade Count:8
Comparative Tracking Index 125 - 600 V125 - 600 VAverage value: 419 V Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 50.0 µm/m-°C5.56 - 27.8 µin/in-°FAverage value: 27.9 µm/m-°C Grade Count:9
CTE, linear, Transverse to Flow 32.0 - 80.0 µm/m-°C17.8 - 44.4 µin/in-°FAverage value: 56.0 µm/m-°C Grade Count:7
Specific Heat Capacity 1.47 - 1.47 J/g-°C
@Temperature 260 - 260 °C
0.351 - 0.351 BTU/lb-°F
@Temperature 500 - 500 °F
Average value: 1.47 J/g-°C Grade Count:1
Thermal Conductivity 0.360 - 0.360 W/m-K
@Temperature 260 - 260 °C
2.50 - 2.50 BTU-in/hr-ft²-°F
@Temperature 500 - 500 °F
Average value: 0.360 W/m-K Grade Count:1
Melting Point 200 - 254 °C392 - 489 °FAverage value: 225 °C Grade Count:21
Maximum Service Temperature, Air 75.0 - 210 °C167 - 410 °FAverage value: 146 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 190 - 228 °C374 - 442 °FAverage value: 221 °C Grade Count:27
Deflection Temperature at 1.8 MPa (264 psi) 193 - 226 °C379 - 439 °FAverage value: 211 °C Grade Count:39
Vicat Softening Point 210 - 225 °C410 - 437 °FAverage value: 216 °C Grade Count:11
Glass Transition Temp, Tg 55.0 - 73.0 °C131 - 163 °FAverage value: 59.5 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:35
Flame Spread 27.0 - 100 mm/min1.06 - 3.94 in/minAverage value: 58.5 mm/min Grade Count:4
Oxygen Index 20.0 %20.0 %Average value: 20.0 % Grade Count:5
Glow Wire Test 650 - 750 °C1200 - 1380 °FAverage value: 718 °C Grade Count:7
 
Processing PropertiesMetricEnglishComments
Processing Temperature 75.0 - 270 °C167 - 518 °FAverage value: 200 °C Grade Count:5
Melt Temperature 220 - 300 °C428 - 572 °FAverage value: 260 °C Grade Count:16
Mold Temperature 30.0 - 130 °C86.0 - 266 °FAverage value: 80.2 °C Grade Count:18
Drying Temperature 80.0 - 140 °C176 - 284 °FAverage value: 119 °C Grade Count:16
Moisture Content 0.0200 - 0.0800 %0.0200 - 0.0800 %Average value: 0.0409 % Grade Count:11
Injection Pressure 60.0 - 103 MPa8700 - 15000 psiAverage value: 83.7 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled

O3215 / 78175

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.