Description: Optibent® is a well selected, high-quality, activated and organically modified layered silicate product which creates moderate thixotropic properties. In flow able systems (floorings, screeds) Optibent® 940 gives an excellent anti-settling effect. This prevents phase separation of coarse sand particles respectively bleeding in screeds after application. Applications: - Self Leveling Compounds
- Smoothing Mortars
- Self Leveling Screeds
Information provided by Southern Clay Products |