MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Feature: Injection Molding, PA66+GF10%, Halogen Free Flame Retardant

Application: Connectors

CAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Water Absorption 0.70 %
@Temperature 23.0 °C,
Time 86400 sec
0.70 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.0900.090Injection Molding
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cm
@Thickness 3.20 mm
0.0070 - 0.012 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 95.6 MPa
@Thickness 3.20 mm
13900 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 5.0 %
@Thickness 3.20 mm
5.0 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 142 MPa
@Thickness 6.40 mm
20600 psi
@Thickness 0.252 in
2.8mm/min; ASTM D790
Flexural Modulus 4.90 GPa
@Thickness 6.40 mm
711 ksi
@Thickness 0.252 in
2.8mm/min; ASTM D790
Izod Impact, Notched 0.392 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.735 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C38.9 µin/in-°FASTM D696
Melting Point 260 °C500 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
@Thickness 6.40 mm
450 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 65.0 °C
@Thickness 0.750 - 0.820 mm
149 °F
@Thickness 0.0295 - 0.0323 in
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 - 0.820 mm
149 °F
@Thickness 0.0295 - 0.0323 in
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.750 - 0.820 mm
149 °F
@Thickness 0.0295 - 0.0323 in
Flammability, UL94 V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 275 °C509 - 527 °FInjection Molding
Middle Barrel Temperature 270 - 280 °C518 - 536 °FInjection Molding
Front Barrel Temperature 270 - 285 °C518 - 545 °FInjection Molding
Nozzle Temperature 270 - 280 °C518 - 536 °FInjection Molding
Melt Temperature 270 - 290 °C518 - 554 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °FInjection Molding
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOL GP3156F Flame Retardant PP
Techmer ES HiFill® PA6/6 GF10 IM L BK 10% Glass Filled
LG Chemical LUMID GP1300A(W) PA6, High Viscosity
LG Chemical LUMID GP1300AP PA6, Plasticized
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose

PLAY171 / 148181

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.