MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Molybdenum, Mo; Soft
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Pure Element

Material Notes: Arc cast, hot worked, and recrystallized at 1100ºC for 1h

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 10.2 g/cc0.368 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 200200
Tensile Strength, Ultimate 485 - 550 MPa70300 - 79800 psi
Tensile Strength, Yield 415 - 450 MPa
@Strain 0.2 %
60200 - 65300 psi
@Strain 0.2 %
Elongation at Break 30 - 40 %30 - 40 %
Modulus of Elasticity 325 GPa47100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000570 ohm-cm0.00000570 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.10 µm/m-°C2.83 µin/in-°F
Specific Heat Capacity 0.251 J/g-°C0.0600 BTU/lb-°F
Thermal Conductivity 137 W/m-K951 BTU-in/hr-ft²-°F
Boiling Point 4639 °C8382 °F
 
Processing PropertiesMetricEnglishComments
Recrystallization Temperature 1100 °C2010 °F
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 99.95 %99.95 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Molybdenum, Mo; Hard
RTP Company RTP 200F MS 2  Nylon 12 (PA 12) Molybdenum Disulfide 2%
Molybdenum Carbide, Mo2C
RTP Company RTP 800 MS 1 Acetal (POM), Molybdenum Disulfide
Molybdenum, Mo, Stress Relieved

MRMo41 / 100363

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.