MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 20% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.37 g/cc0.0434 - 0.0495 lb/in³Average value: 1.26 g/cc Grade Count:40
Water Absorption 1.30 - 8.00 %1.30 - 8.00 %Average value: 3.58 % Grade Count:25
Moisture Absorption at Equilibrium 1.80 - 3.00 %1.80 - 3.00 %Average value: 2.35 % Grade Count:11
 2.30 - 2.30 %
@Temperature 70.0 - 70.0 °C
2.30 - 2.30 %
@Temperature 158 - 158 °F
Average value: 2.30 % Grade Count:2
Water Absorption at Saturation 5.00 - 8.00 %5.00 - 8.00 %Average value: 6.60 % Grade Count:20
Linear Mold Shrinkage 0.00100 - 0.0140 cm/cm0.00100 - 0.0140 in/inAverage value: 0.00594 cm/cm Grade Count:22
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm0.00100 - 0.0100 in/inAverage value: 0.00518 cm/cm Grade Count:20
Melt Flow 3.00 - 157 g/10 min3.00 - 157 g/10 minAverage value: 80.6 g/10 min Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 77.0 - 88.077.0 - 88.0Average value: 83.0 Grade Count:10
Ball Indentation Hardness 75.0 - 210 MPa10900 - 30500 psiAverage value: 146 MPa Grade Count:15
Tensile Strength, Ultimate 46.0 - 180 MPa6670 - 26100 psiAverage value: 106 MPa Grade Count:33
 52.0 - 53.0 MPa
@Temperature -40.0 - -40.0 °C
7540 - 7690 psi
@Temperature -40.0 - -40.0 °F
Average value: 52.5 MPa Grade Count:1
Tensile Strength, Yield 12.0 - 95.0 MPa1740 - 13800 psiAverage value: 61.2 MPa Grade Count:6
Elongation at Break 2.00 - 10.0 %2.00 - 10.0 %Average value: 4.59 % Grade Count:31
 1.70 - 2.10 %
@Temperature -40.0 - -40.0 °C
1.70 - 2.10 %
@Temperature -40.0 - -40.0 °F
Average value: 1.90 % Grade Count:1
Elongation at Yield 3.00 - 10.0 %3.00 - 10.0 %Average value: 5.75 % Grade Count:8
Modulus of Elasticity 2.70 - 9.03 GPa392 - 1310 ksiAverage value: 5.33 GPa Grade Count:38
 4.06 - 4.88 GPa
@Temperature -40.0 - -40.0 °C
589 - 708 ksi
@Temperature -40.0 - -40.0 °F
Average value: 4.47 GPa Grade Count:1
Flexural Yield Strength 147 - 210 MPa21300 - 30500 psiAverage value: 180 MPa Grade Count:7
Flexural Modulus 4.90 - 8.32 GPa711 - 1210 ksiAverage value: 6.33 GPa Grade Count:7
Izod Impact, Notched (ISO) 5.00 - 16.0 kJ/m²2.38 - 7.61 ft-lb/in²Average value: 9.40 kJ/m² Grade Count:6
Charpy Impact Unnotched 2.50 - 10.1 J/cm²11.9 - 48.0 ft-lb/in²Average value: 5.88 J/cm² Grade Count:36
 2.50 - 7.98 J/cm²
@Temperature -40.0 - -20.0 °C
11.9 - 38.0 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 4.98 J/cm² Grade Count:25
Charpy Impact, Notched 0.400 - 2.52 J/cm²1.90 - 12.0 ft-lb/in²Average value: 1.00 J/cm² Grade Count:35
 0.273 - 1.008 J/cm²
@Temperature -30.0 - -20.0 °C
1.30 - 4.797 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.555 J/cm² Grade Count:24
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+15 ohm-cm1.00e+9 - 1.00e+15 ohm-cmAverage value: 1.89e+14 ohm-cm Grade Count:28
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 6.69e+13 ohm Grade Count:14
Dielectric Strength 25.0 - 40.0 kV/mm635 - 1020 kV/inAverage value: 31.9 kV/mm Grade Count:24
Dissipation Factor 0.0200 - 0.03000.0200 - 0.0300Average value: 0.0233 Grade Count:3
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 577 V Grade Count:25
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 - 45.0 µm/m-°C11.0 - 25.0 µin/in-°FAverage value: 29.0 µm/m-°C Grade Count:18
CTE, linear, Transverse to Flow 75.0 - 110 µm/m-°C41.7 - 61.1 µin/in-°FAverage value: 93.7 µm/m-°C Grade Count:14
Melting Point 195 - 310 °C383 - 590 °FAverage value: 256 °C Grade Count:27
Maximum Service Temperature, Air 90.0 - 260 °C194 - 500 °FAverage value: 170 °C Grade Count:14
Deflection Temperature at 0.46 MPa (66 psi) 168 - 215 °C334 - 419 °FAverage value: 202 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 114 - 270 °C237 - 518 °FAverage value: 218 °C Grade Count:27
Deflection Temperature at 8.0 MPa 60.0 - 100 °C140 - 212 °FAverage value: 80.4 °C Grade Count:14
Minimum Service Temperature, Air 90.0 - 100 °C194 - 212 °FAverage value: 92.0 °C Grade Count:5
Flammability, UL94 HB - V-0HB - V-0Grade Count:20
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 857 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 310 °C437 - 590 °FAverage value: 272 °C Grade Count:8
Mold Temperature 50.0 - 100 °C122 - 212 °FAverage value: 75.7 °C Grade Count:7
Drying Temperature 80.0 °C176 °FAverage value: 80.0 °C Grade Count:4
Moisture Content 0.150 %0.150 %Average value: 0.150 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
Overview of materials for Nylon 66/6
Overview of materials for Nylon 66, 20% Glass Fiber Filled
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced

O2492 / 77993

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.