MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD 3482-1 Liquid Crystal Polymer (LCP); Carbon Fiber - Electrically Conductive - (Preliminary Data Sheet)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Carbon Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D 792
Additive Loading 15 %15 %Primary Additive
Linear Mold Shrinkage 0.0010 cm/cm
@Thickness 3.20 mm
0.0010 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 186 MPa27000 psiASTM D 638
Elongation at Break 3.0 %3.0 %ASTM D 638
Tensile Modulus 17.2 GPa2500 ksiASTM D 638
Flexural Strength 241 MPa35000 psiASTM D 790
Flexural Modulus 14.5 GPa2100 ksiASTM D 790
Izod Impact, Notched 2.67 J/cm
@Thickness 3.20 mm
5.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 7.47 J/cm
@Thickness 3.20 mm
14.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmASTM D 257
Surface Resistance <= 10000 ohm<= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C430 °FASTM D 648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 302 °C520 - 575 °F
Mold Temperature 37.8 - 93.3 °C100 - 200 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
Injection Pressure 34.5 - 82.7 MPa5000 - 12000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
RTP Company RTP 3483-1 Liquid Crystal Polymer (LCP), Carbon Fiber
Celanese Vectra® C130 Liquid Crystal Polymer (LCP), 30% Glass Reinforced
RTP Company RTP 3499-4 X 91192 A Liquid Crystal Polymer (LCP), High Heat Encapsulation Grade
RTP Company RTP 3400 G-430 Liquid Crystal Polymer (LCP), Glass Fiber - UL94 V-0

PQZRA38149 / 205900

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.