MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Fortron 1140L6 is an easier flow version of Fortron 1140L4. It offers essentially the same characteristics of 1140L4. Especially used for thin walled parts with long flow lengths. Applications made of this grade include components for pumps and electronics.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
Density 1.65 g/cc0.0596 lb/in³ISO 1183
Water Absorption 0.020 %
@Temperature 22.8 °C
0.020 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Water Absorption at Saturation 0.020 %0.020 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 19 g/10 min19 g/10 minASTM D1238
Spiral Flow 21.5 cm8.46 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ISO 2039-2
 100100ASTM D785
Tensile Strength at Break 195 MPa28300 psi5mm/min; ISO 527-2/1A
 200 MPa29000 psiASTM D638
Elongation at Break 1.9 %1.9 %5mm/min; ISO 527-2/1A
 2.0 %2.0 %ASTM D638
Tensile Modulus 14.7 GPa2130 ksi50mm/min; ISO 527-2/1A
Flexural Strength 276 MPa40000 psiASTM D790
 285 MPa41300 psiISO 178
Flexural Modulus 13.8 GPa2000 ksiASTM D790
 14.5 GPa2100 ksiISO 178
Izod Impact, Notched 1.01 J/cm1.90 ft-lb/inASTM D256
Izod Impact, Unnotched 5.87 J/cm11.0 ft-lb/inASTM D256
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 34.0 kJ/m²
@Temperature 23.0 °C
16.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 5.30 J/cm²25.2 ft-lb/in²ISO 179/1eU
 5.30 J/cm²
@Temperature -30.0 °C
25.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
ASTM D150
 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150
 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 15.4 kV/mm390 kV/inshort term; ASTM D149
 28.0 kV/mm711 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 134 sec134 secASTM D495
Comparative Tracking Index 125 V125 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C14.4 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 42.0 µm/m-°C23.3 µin/in-°FISO 11359-2
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FASTM D648
 270 °C518 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 215 °C419 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °Fcavity
 330 - 340 °C626 - 644 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 290 - 300 °C554 - 572 °F
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 330 - 340 °C626 - 644 °F
Zone 4 330 - 340 °C626 - 644 °F
Die Temperature 310 - 330 °C590 - 626 °F
Melt Temperature 310 - 340 °C590 - 644 °FISO 294
 330 - 340 °C626 - 644 °F
Mold Temperature 135 - 160 °C275 - 320 °FISO 294
Drying Temperature 130 - 140 °C266 - 284 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 50.0 - 100 MPa7250 - 14500 psi
Hold Pressure 30.0 - 70.0 MPa4350 - 10200 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  50 rpm
@Diameter 55.0 mm
50 rpm
@Diameter 2.17 in
 75 rpm
@Diameter 40.0 mm
75 rpm
@Diameter 1.57 in
 120 rpm
@Diameter 25.0 mm
120 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedfast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35
Celanese Thermx® CG933 NC010 PCT
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Celanese Zenite® 6130 BK010 LCP, 30% glass reinforced (Extended Tabular Temperature Data)

PHCQ272 / 178727

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.