MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Celanex® 3300-2 PBT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outstanding processability and good chemical resistance. Celanex 3300-2 is a high flow material that contains an internal lubricant.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccASTM D792
Density 1.53 g/cc0.0553 lb/in³ISO 1183
Water Absorption 0.070 %
@Temperature 22.8 °C
0.070 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Viscosity Test 74 cm³/g0.74 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D955
 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cm0.0070 - 0.011 in/inISO 294-4
Melt Flow 16 g/10 min16 g/10 minASTM D1238
 17 g/10 min
@Load 2.16 kg,
Temperature 250 °C
17 g/10 min
@Load 4.76 lb,
Temperature 482 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ISO 2039-2
Tensile Strength at Break 130 MPa18900 psi5mm/min; ISO 527-2/1A
 134 MPa19500 psiASTM D638
 61.4 MPa
@Temperature 121 °C
8900 psi
@Temperature 250 °F
ASTM D638
 77.57 MPa
@Temperature 80.0 °C
11250 psi
@Temperature 176 °F
ASTM D638
 159 MPa
@Temperature 0.000 °C
23000 psi
@Temperature 32.0 °F
ASTM D638
 190 MPa
@Temperature -40.0 °C
27500 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
 2.5 %2.5 %5mm/min; ISO 527-2/1A
 1.9 %
@Temperature 0.000 °C
1.9 %
@Temperature 32.0 °F
ASTM D638
 1.9 %
@Temperature 4.44 °C
1.9 %
@Temperature 40.0 °F
ASTM D638
 3.9 %
@Temperature 80.0 °C
3.9 %
@Temperature 176 °F
ASTM D638
 4.3 %
@Temperature 121 °C
4.3 %
@Temperature 250 °F
ASTM D638
Tensile Modulus 9.20 GPa1330 ksi50mm/min; ISO 527-2/1A
 9.65 GPa1400 ksiASTM D638
 3.76 GPa
@Temperature 121 °C
545 ksi
@Temperature 250 °F
ASTM D638
 4.83 GPa
@Temperature 80.0 °C
700 ksi
@Temperature 176 °F
ASTM D638
 10.5 GPa
@Temperature 0.000 °C
1520 ksi
@Temperature 32.0 °F
ASTM D638
 11.0 GPa
@Temperature -40.0 °C
1600 ksi
@Temperature -40.0 °F
ASTM D638
Flexural Strength 193 MPa28000 psiASTM D790
 210 MPa30500 psiISO 178
Flexural Modulus 8.27 GPa1200 ksiASTM D790
 9.70 GPa1410 ksiISO 178
Izod Impact, Notched 0.908 J/cm1.70 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 7.50 kJ/m²3.57 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 4.60 J/cm²21.9 ft-lb/in²ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²4.04 ft-lb/in²ISO 179/1eA
 0.850 J/cm²
@Temperature -30.0 °C
4.04 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
ASTM D150
 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 60250
 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm560 kV/inshort term; ASTM D149
 31.0 kV/mm787 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 0.0022
@Frequency 100 Hz
0.0022
@Frequency 100 Hz
IEC 60250
 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 425 V425 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-2,-3
 225 °C437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FISO 75-1, -2
 228 °C442 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-1, -2
 206 °C403 °FASTM D648
Deflection Temperature at 8.0 MPa 150 °C302 °FISO 75-1, -2
Vicat Softening Point 220 °C428 °FISO 306
Glass Transition Temp, Tg 60.0 °C140 °FISO 11357-1,-2,-3
Flammability, UL94 HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
Oxygen Index 20 %20 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 65.0 - 93.0 °C149 - 199 °Fcavity
 250 - 260 °C482 - 500 °Fhot runner
Feed Temperature 230 - 240 °C446 - 464 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 235 - 260 °C455 - 500 °F
 260 °C500 °FISO 294
Mold Temperature 82.0 °C180 °FISO 294
Injection Velocity 300 mm/sec11.8 in/secISO 294
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Hold Pressure 48.0 MPa6960 psiISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Novaduran® 5010GN6-30M8X Polybutylene Terephthalate
Mitsubishi Novaduran® 5010GN6-30T Polybutylene Terephthalate
Celanese Crastin® SK603 BK851 PBT-GF20
DuPont Mobility and Materials Delrin® 500P NC010 POM
Celanese Celanex® 3300-2FC PBT, 30% Glass Reinforced

PHCQ047 / 178502

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.