MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled; Polyphenylene Ether, Heat Resistant

Material Notes: Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass Reinforced

Features: • Bromine Free • Chlorine Free
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219; Polyphenylene Ether + PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inASTM D955
Melt Flow 1.0 - 8.0 g/10 min
@Load 11.6 kg,
Temperature 250 °C
1.0 - 8.0 g/10 min
@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 110 MPa16000 psiASTM D638
Tensile Strength, Yield 117 MPa17000 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Strength 131 MPa19000 psiASTM D790
Flexural Modulus 7.24 GPa1050 ksiASTM D790
Izod Impact, Notched  0.747 J/cm
@Temperature -40.0 °C
1.40 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.961 J/cm
@Temperature 22.8 °C
1.80 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Charpy Impact, Notched 0.777 J/cm²
@Temperature 22.8 °C
3.70 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C265 °FASTM D648
UL RTI, Electrical  65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-1 - 5VA
@Thickness 1.60 mm
V-1 - 5VA
@Thickness 0.0630 in
 V-1 - 5VA
@Thickness 3.00 mm
V-1 - 5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 299 °C480 - 570 °F
Middle Barrel Temperature 260 - 304 °C500 - 580 °F
Front Barrel Temperature 271 - 310 °C520 - 590 °F
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 71.1 - 98.9 °C160 - 210 °F
Drying Temperature 104 - 110 °C220 - 230 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00254 cm0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO
LNP NORYL® PX2926 Polyphenylene Ether + Polystyrene, Filled
Mitsubishi Iupiace® LN30 m-Polyphenylene Ether (m-PPE)

PPOLYQ218 / 160739

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.