MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sichuan Deyang Haton® hs1237B Polyphenylene Sulfide Coating
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) Coating Resin

Material Notes: Suspension; anti-corrosion

Information provided by Sichuan Deyang Chemical Co., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.020 %<= 0.020 %GB/T 1034-2008
 
Mechanical PropertiesMetricEnglishComments
Impact NBNBGb1720
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 - 220 °C356 - 428 °F
 
Descriptive Properties
Chemical ResistanceAmmonia, 40%< 0.001 mg/h*cm2
 Hydrochloric Acid, 40%< 0.001 mg/h*cm2
 Sodium Chloride, 5%< 0.001 mg/h*cm2
 Sodium Hydroxide, 50%< 0.001 mg/h*cm2
 Sulfuric Acid, 40%< 0.001 mg/h*cm2
Heat Resistance, g0.21260°C, 500 h
Pencil Hardness>2 HGB/T6739

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sichuan Deyang Haton® hs2331B Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hs23310 Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hs12370 Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hp23310 Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hp12370 Polyphenylene Sulfide Coating

PSICHU930 / 156171

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.