MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Low Density Polyethylene

Customer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 2.5 g/10 min2.5 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psi2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psi2 in per min; ASTM D882
Film Elongation at Break, MD 500 %500 %2 in per min; ASTM D882
Film Elongation at Break, TD 500 %500 %2 in per min; ASTM D882
Elmendorf Tear Strength MD 100 g100 gASTM D1922
Elmendorf Tear Strength TD 300 g300 gASTM D1922
Dart Drop Test 100 g0.221 lbASTM D1709
Film Tensile Strength at Break, MD 27.0 MPa3920 psi2 in per min; ASTM D882
Film Tensile Strength at Break, TD 22.0 MPa3190 psi2 in per min; ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Gloss 91 %91 %45°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin
Petromont 2100 Medium Density Polyethylene Resin
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Braskem LL218 Cast Film Extrusion Linear Low Density Polyethylene

PCHEVP01 / 20341

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.