MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride
Categories: Ceramic; Nitride

Material Notes: Uniform, large sized pressed sintered aluminum nitride.

Key Words: AlN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.24 g/cc0.117 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 320 GPa46400 ksi
Flexural Strength 356 MPa51600 psi
Poissons Ratio 0.240.24
Shear Modulus 129 GPa18700 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.10e+13 ohm-cm3.10e+13 ohm-cm
Dielectric Constant 8.9
@Frequency 1e+6 Hz
8.9
@Frequency 1e+6 Hz
Dielectric Strength 18.7 kV/mm475 kV/in
Dissipation Factor 0.00026
@Frequency 1e+6 Hz
0.00026
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.90 µm/m-°C2.17 µin/in-°F
Thermal Conductivity 86.0 W/m-K597 BTU-in/hr-ft²-°F
 
Descriptive Properties
Purity> 99.0% (Al + N)
 > 99.9% (Al + N + O)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride
Aluminum Nitride, AlN
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride
American Elements Aluminum Nitride Nanoparticles
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable

CTOKUY91 / 104643

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.