MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of strength, stiffness and excellent moldability/surface aesthetics. It is also available in heat stabilized (Ultramid 8333G HI HS) and/or pigmented versions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption 0.90 %0.90 %24 hour; ISO Test
 5.5 %5.5 %ISO 62
Moisture Absorption at Equilibrium 1.5 %1.5 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM Test
Tensile Strength at Break 150 MPa21800 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 140 MPa20300 psi5mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527
 3.0 %3.0 %0.2 in/min; ASTM Test
Tensile Modulus 9.10 GPa1320 ksi1mm/min; ISO 527
Flexural Strength 210 MPa30500 psiISO Data
 240 MPa34800 psiASTM Test
Flexural Modulus 7.50 GPa1090 ksiISO Data
 8.14 GPa1180 ksiASTM Test
Izod Impact, Notched 1.05 J/cm
@Temperature -40.0 °C
1.97 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 2.10 J/cm
@Thickness 3.17 mm
3.93 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 19.0 kJ/m²9.04 ft-lb/in²ISO Test
 13.0 kJ/m²
@Temperature -40.0 °C
6.19 ft-lb/in²
@Temperature -40.0 °F
ISO Test
Charpy Impact Unnotched 7.10 J/cm²33.8 ft-lb/in²ISO 179
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75
 210 °C410 °FASTM Test
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)

PBASF9205 / 84969

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.