MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Feature: Injection Molding, PA6+GF25%, Flame Retardant

Application: IT/OA (Micro Switch)

CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
Water Absorption 0.70 %
@Temperature 23.0 °C,
Time 86400 sec
0.70 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0090 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength, Yield 162 MPa
@Thickness 3.20 mm
23500 psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.20 mm
3.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 221 MPa
@Thickness 3.20 mm
32000 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 8.83 GPa
@Thickness 3.20 mm
1280 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 1.08 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.02 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 21.0 kV/mm
@Thickness 1.00 mm
533 kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance 90 sec90 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 V
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 41.0 µm/m-°C22.8 µin/in-°FASTM D696
Melting Point 220 °C428 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
@Thickness 6.40 mm
374 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  120 °C
@Thickness >=0.750 mm
248 °F
@Thickness >=0.0295 in
 120 °C
@Thickness >=1.50 mm
248 °F
@Thickness >=0.0591 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  110 °C
@Thickness >=0.750 mm
230 °F
@Thickness >=0.0295 in
 110 °C
@Thickness >=1.50 mm
230 °F
@Thickness >=0.0591 in
 110 °C
@Thickness >=3.00 mm
230 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  115 °C
@Thickness >=0.750 mm
239 °F
@Thickness >=0.0295 in
 115 °C
@Thickness >=1.50 mm
239 °F
@Thickness >=0.0591 in
 115 °C
@Thickness >=3.00 mm
239 °F
@Thickness >=0.118 in
Flammability, UL94  V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 260 °C446 - 500 °FInjection Molding
Middle Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Front Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Nozzle Temperature 240 - 270 °C464 - 518 °FInjection Molding
Melt Temperature 240 - 265 °C464 - 509 °FInjection Molding
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, DRY
Domo TECHNYL® B 50 H1 PA66/6, DRY
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant

PLAY174 / 148184

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.